Spin 2
Negative Resist Spinner
- Two Spinners
- Maximum speed of 10,000 rpm
- User friendly programmable interface
- Programmable step functions (up to 10 steps per recipe)
- Programmable process control
- Wafer sizes from pieces through
-300mm capable bowl sizes